Parameter   Unit   Value  
     
 Thickness of the Coating  mm  0,5 - 0,8 
 Specific Electrical Resistivity  Ω.µm  0,07 – 0,10 
 Gas impermeability at 900 °C  h   above 50
 Temperature when Decomposition Process starts   °C   above 1850 